China GH136 Alloy is a nickel-based superalloy with high strength and excellent
China GH136 Alloy is a nickel-based superalloy with high strength and excellent

  1. China GH136 Alloy is a nickel-based superalloy with high strength and excellent
  2. China GH136 Alloy is a nickel-based superalloy with high strength and excellent

GH136 Alloy is a nickel-based superalloy with high strength and excellent

  1. MOQ: 100KG
  2. Price: Price is negotiated based on the required specifications and quantity
  3. Get Latest Price
Payment Terms Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability 5000 tons per month
Delivery Time 5-8 working days, depending on the parameters required for negotiation
Packaging Details Standard export packaging, or packaging as required
Density ~8.8 g/cm³ (0.317 lb/in³)
Melting Point ~1300-1400°C (2370-2550°F)
Tensile Strength ~900 MPa (130 ksi)
Yield Strength ~700 MPa (102 ksi)
Elongation ~15%
Thermal Conductivity ~13 W/m·K (9 BTU·in/hr·ft²·°F)
Modulus of Elasticity ~210 GPa (30 x 10³ ksi)
Corrosion Resistance Good oxidation and corrosion resistance at high temperatures
Brand Name Zhonggong Special Metallurgy
Model Number GH136 Alloy
Place of Origin China
Certification ISO Certificate

View Detail Information

Contact Now Ask for best deal
Get Latest Price Request a quote
  1. Product Details
  2. Company Details

Product Specification

Payment Terms Payment Terms: Mainly T/T.. L/C, D/A, D/P, Supply Ability 5000 tons per month
Delivery Time 5-8 working days, depending on the parameters required for negotiation Packaging Details Standard export packaging, or packaging as required
Density ~8.8 g/cm³ (0.317 lb/in³) Melting Point ~1300-1400°C (2370-2550°F)
Tensile Strength ~900 MPa (130 ksi) Yield Strength ~700 MPa (102 ksi)
Elongation ~15% Thermal Conductivity ~13 W/m·K (9 BTU·in/hr·ft²·°F)
Modulus of Elasticity ~210 GPa (30 x 10³ ksi) Corrosion Resistance Good oxidation and corrosion resistance at high temperatures
Brand Name Zhonggong Special Metallurgy Model Number GH136 Alloy
Place of Origin China Certification ISO Certificate
High Light high strength nickel based alloyshigh strength nickel based superalloy

GH136 Alloy is a high-performance nickel-based superalloy engineered for superior strength and oxidation resistance at elevated temperatures. This alloy is designed to perform reliably in extreme environments, making it suitable for demanding applications in aerospace and high-temperature industrial processes.

Key Properties and Features:

  • High-Temperature Strength: GH136 Alloy maintains excellent mechanical properties, including high tensile strength (~900 MPa or 130 ksi) and yield strength (~700 MPa or 102 ksi), at temperatures up to approximately 1300-1400°C (2370-2550°F). This capability makes it ideal for components exposed to intense heat.
  • Oxidation and Corrosion Resistance: The alloy offers robust resistance to oxidation and high-temperature corrosion, ensuring long-term durability and performance in harsh environments. This feature is crucial for applications in gas turbines, jet engines, and other high-stress applications.
  • Mechanical Properties: Provides good elongation (~15%), which contributes to its ability to withstand mechanical stress without compromising integrity.
  • Thermal Conductivity: With a thermal conductivity of approximately 13 W/m·K (9 BTU·in/hr·ft²·°F), GH136 effectively manages heat dissipation, which is important in high-performance systems.
  • Applications: Commonly used in aerospace components, gas turbines, and other high-temperature structural parts where high strength and resistance to thermal degradation are required.

GH136 Alloy’s combination of high strength, oxidation resistance, and thermal stability ensures it is a reliable choice for advanced engineering applications demanding exceptional performance under extreme conditions.

 

Here’s a composition table for GH136 Alloy:

Element Composition Range (%)
Nickel (Ni) 60.0 - 65.0
Chromium (Cr) 14.0 - 16.0
Cobalt (Co) 8.0 - 10.0
Molybdenum (Mo) 3.0 - 5.0
Iron (Fe) ≤ 6.0
Titanium (Ti) 1.0 - 2.0
Aluminum (Al) 1.0 - 2.0
Carbon (C) ≤ 0.10
Manganese (Mn) ≤ 0.5
Silicon (Si) ≤ 0.5
Sulfur (S) ≤ 0.01

These values provide general guidelines. For precise specifications or applications, consult specific standards or suppliers.

 

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Seller,Other

  • Year Established:

    2022

  • Total Annual:

    1000000-1500000

  • Employee Number:

    100~200

  • Ecer Certification:

    Verified Supplier

Main Products Stainless Steel Series304,304L,321,316L,317L,309s,310s,904L,410,420,430,441,409,436,441,439,630 etc. Duplex stainless steel series 2205,2507  etc. Hastelloy C-276, B-2, C-2000, etc. Nickel-based alloy series Inconel625,718,Incoloy825,800H,Monel400, etc. High temperature alloy ser... Main Products Stainless Steel Series304,304L,321,316L,317L,309s,310s,904L,410,420,430,441,409,436,441,439,630 etc. Duplex stainless steel series 2205,2507  etc. Hastelloy C-276, B-2, C-2000, etc. Nickel-based alloy series Inconel625,718,Incoloy825,800H,Monel400, etc. High temperature alloy ser...

+ Read More

Get in touch with us

  • Reach Us
  • Jiangsu Zhonggongte Metallurgical Technology Co., Ltd.
  • New South Stainless Steel Trading Market, Fangcheng Avenue, Wuxi City, Jiangsu Province, 12-101.
  • https://www.hastelloy-alloys.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement