China GH600 Alloy: Nickel-based superalloy with high strength, excellent oxidation
China GH600 Alloy: Nickel-based superalloy with high strength, excellent oxidation

  1. China GH600 Alloy: Nickel-based superalloy with high strength, excellent oxidation
  2. China GH600 Alloy: Nickel-based superalloy with high strength, excellent oxidation

GH600 Alloy: Nickel-based superalloy with high strength, excellent oxidation

  1. MOQ: 100KG
  2. Price: Price is negotiated based on the required specifications and quantity
  3. Get Latest Price
Payment Terms Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability 5000 tons per month
Delivery Time 5-8 working days, depending on the parameters required for negotiation
Packaging Details Standard export packaging, or packaging as required
Material Type Nickel-based Superalloy
Density ~8.4 g/cm³
Tensile Strength ~750 MPa
Yield Strength ~600 MPa
Temperature Range Up to 1100°C (2012°F)
Oxidation Resistance Excellent
Corrosion Resistance Good
Applications Aerospace, industrial gas turbines, exhaust systems
Heat Treatment Solution treated and aged
Form Bars, sheets, forgings, and custom shapes
Brand Name Zhonggong Special Metallurgy
Model Number GH600 Alloy
Place of Origin China
Certification ISO Certificate

View Detail Information

Contact Now Ask for best deal
Get Latest Price Request a quote
  1. Product Details
  2. Company Details

Product Specification

Payment Terms Payment Terms: Mainly T/T.. L/C, D/A, D/P, Supply Ability 5000 tons per month
Delivery Time 5-8 working days, depending on the parameters required for negotiation Packaging Details Standard export packaging, or packaging as required
Material Type Nickel-based Superalloy Density ~8.4 g/cm³
Tensile Strength ~750 MPa Yield Strength ~600 MPa
Temperature Range Up to 1100°C (2012°F) Oxidation Resistance Excellent
Corrosion Resistance Good Applications Aerospace, industrial gas turbines, exhaust systems
Heat Treatment Solution treated and aged Form Bars, sheets, forgings, and custom shapes
Brand Name Zhonggong Special Metallurgy Model Number GH600 Alloy
Place of Origin China Certification ISO Certificate
High Light high strength nickel based alloyshigh strength nickel based superalloy

GH600 Alloy is a high-performance nickel-based superalloy specifically designed for applications requiring exceptional strength and durability at high temperatures. It provides outstanding mechanical properties, thermal stability, and oxidation resistance, making it ideal for severe environments.

Key Features:

  • Composition: Predominantly nickel with chromium, molybdenum, titanium, and aluminum. These elements contribute to the alloy’s high strength and resistance to heat and corrosion.
  • Temperature Resistance: Effective in applications up to 1100°C (2012°F), maintaining mechanical integrity and stability.
  • Mechanical Properties: Offers high tensile and yield strength, ensuring reliability under extreme stress conditions.
  • Oxidation and Corrosion Resistance: Excellent resistance to oxidation and good resistance to corrosion, extending the life of components.
  • Applications: Commonly used in aerospace engines, industrial gas turbines, and high-temperature exhaust systems.
  • Heat Treatment: Can be heat-treated to achieve optimal strength and performance characteristics, providing versatility in manufacturing.

GH600 Alloy's advanced properties make it suitable for demanding aerospace and industrial applications, ensuring long-term performance and reliability in challenging environments.

 

Here’s a detailed composition table for GH600 Alloy:

Element Composition (%)
Nickel (Ni) Balance
Chromium (Cr) 14.0 - 16.0
Molybdenum (Mo) 4.0 - 5.0
Titanium (Ti) 1.8 - 2.5
Aluminum (Al) 1.0 - 1.5
Iron (Fe) ≤ 4.0
Carbon (C) ≤ 0.08
Silicon (Si) ≤ 0.50
Manganese (Mn) ≤ 0.50
Boron (B) ≤ 0.01

These values provide a general guideline, but exact specifications can vary slightly based on the manufacturer's standards and requirements.

 

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Seller,Other

  • Year Established:

    2022

  • Total Annual:

    1000000-1500000

  • Employee Number:

    100~200

  • Ecer Certification:

    Verified Supplier

Main Products Stainless Steel Series304,304L,321,316L,317L,309s,310s,904L,410,420,430,441,409,436,441,439,630 etc. Duplex stainless steel series 2205,2507  etc. Hastelloy C-276, B-2, C-2000, etc. Nickel-based alloy series Inconel625,718,Incoloy825,800H,Monel400, etc. High temperat... Main Products Stainless Steel Series304,304L,321,316L,317L,309s,310s,904L,410,420,430,441,409,436,441,439,630 etc. Duplex stainless steel series 2205,2507  etc. Hastelloy C-276, B-2, C-2000, etc. Nickel-based alloy series Inconel625,718,Incoloy825,800H,Monel400, etc. High temperat...

+ Read More

Get in touch with us

  • Reach Us
  • Jiangsu Zhonggongte Metallurgical Technology Co., Ltd.
  • New South Stainless Steel Trading Market, Fangcheng Avenue, Wuxi City, Jiangsu Province, 12-101.
  • https://www.hastelloy-alloys.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement