Payment Terms | T/T |
Supply Ability | More than 1 million |
Delivery Time | 30day |
Packaging Details | As the customer required |
Emphasize | Injection Molding Solution |
Place of Origin | CHINA |
Brand Name | OEM |
Certification | ISO |
View Detail Information
Explore similar products
OEM Injection Molding Solution Regular Daily Maintenance
Plastic Manufacturing Made Easy with Smooth Surface Finish Injection Molding
Achieve Optimal Mold Temperature with Injection Molding Solution
Smooth Surface Finish Injection Molding System with Short Lead Time
Product Specification
Payment Terms | T/T | Supply Ability | More than 1 million |
Delivery Time | 30day | Packaging Details | As the customer required |
Emphasize | Injection Molding Solution | Place of Origin | CHINA |
Brand Name | OEM | Certification | ISO |
High Light | Fuse Connection Injection Molding Solution ,Injection Molding Solution ,Injection Molding Solution ISO |
The Reason And Countermeasure Analysis Of Product Fuse Connection
1. Welding line
Weld line, also known as weld mark and water clip, is a thin line produced by cooling the front section of the molten resin in the original H different, and failing to fully fuse in combination. Strictly speaking, almost all products have fuse wiring, it is difficult to completely eliminate, just try to weaken, or move it to a place where it does not matter
Cause | Cuntermeasure | |
Forming condition |
1. The material temperature is too low 2. Mold temperature is too low 3. Injection molding speed is too low 4. Insufficient injection pressure and retaining pressure 5. Insufficient drying of materials, too much gas |
1. Increase the molding temperature 2. Set the right temperature 3. Increase the speed, but pay attention to poor exhaust 4. Increase stress 5. Powder and dry materials |
Die |
1. Screw back pressure is insufficient 2. Improper gate location and number 3. Mold exhaust is poor
|
1. Increase back pressure 2. Change the location and number 3. Improve the exhaust, reduce the clamping force is conducive to exhaust |
Product Design |
1. The wall thickness is too thin or the wall thickness difference is too large 2. There are too many holes 3. Improper product color designation, metal color boundary to produce fuse line |
1. Avoid it during design 2. Try to reduce the number 3. Change the color or choose the right material |
Material |
1. The influence of material additives 2. Poor material fluidity |
1. Reduce or change additives 2. Improve material mobility |
Other |
1. The influence of release agent 2. The screw check ring is damaged |
1. Try not to use it 2. Replace the check ring |
Company Details
Business Type:
Manufacturer
Year Established:
1997
Total Annual:
18000000-22000000
Employee Number:
1~1000
Ecer Certification:
Site Member
Sun On was founded in 1997. After years of development, we gradually bloomed into a diversified manufacturing factory, with Product Design, Rapid Prototype, Molds Making, Plastic Injection Production, Die Casting Alloy Production and Precision Parts Machining. together with surface fini... Sun On was founded in 1997. After years of development, we gradually bloomed into a diversified manufacturing factory, with Product Design, Rapid Prototype, Molds Making, Plastic Injection Production, Die Casting Alloy Production and Precision Parts Machining. together with surface fini...
Get in touch with us
Leave a Message, we will call you back quickly!