Name | Incoloy Alloy 800H |
Density | 8.0-8.2 g/cm³ |
Melting Point | 1350-1400°C (2460-2550°F) |
Tensile Strength | 520-690 MPa (75,400-100,000 psi) |
Yield Strength (0.2% offset) | 205-310 MPa (29,700-45,000 psi) |
Elongation | 30% min |
Hardness (Brinell) | ≤200 HB |
Electrical Resistivity | 1.08 µΩ·m at 20°C (68°F) |
Brand Name | Zhonggong Special Metallurgy |
Model Number | Incoloy800H nickel-based |
Place of Origin | China |
Certification | ISO Certificate |
View Detail Information
Explore similar products
Incoloy 926 Corrosion Resistant Alloy High Strength UNS N08926 Light Rod And
926 Nickel Based Alloy Steel Rods Excellent Processing Alloy 1.4529 Tubes
Oxidation Resistant Incoloy 800HT Alloy Bar With Enhanced Thermal Stability
8.14g/cm3 Nickel Based Alloy 925 Round Bar Incoloy 925 Alloy
Product Specification
Payment Terms | Payment Terms: Mainly T/T.. L/C, D/A, D/P, | Supply Ability | 5000 tons per month |
Delivery Time | 5-8 working days, depending on the parameters required for negotiation | Packaging Details | Standard export packaging, or packaging as required |
Name | Incoloy Alloy 800H | Density | 8.0-8.2 g/cm³ |
Melting Point | 1350-1400°C (2460-2550°F) | Tensile Strength | 520-690 MPa (75,400-100,000 psi) |
Yield Strength (0.2% offset) | 205-310 MPa (29,700-45,000 psi) | Elongation | 30% min |
Hardness (Brinell) | ≤200 HB | Electrical Resistivity | 1.08 µΩ·m at 20°C (68°F) |
Brand Name | Zhonggong Special Metallurgy | Model Number | Incoloy800H nickel-based |
Place of Origin | China | Certification | ISO Certificate |
High Light | Incoloy 800H nickel based alloy ,nickel based alloy N08810 ,N08810 Round Bar |
High strength Incoloy800H nickel-based alloy round bar N08810 black bar 10-100mm anti-stress corrosion cracking.
Incoloy 800H is a nickel-based high-temperature alloy with good high-temperature strength, oxidation resistance and corrosion resistance. It is widely used in chemical, petrochemical, energy and nuclear energy industries. Its chemical composition is mainly based on nickel, iron and chromium, and also contains a small amount of molybdenum, copper, silicon and other elements. This alloy is usually used in high temperature environments and corrosive media, especially those applications that require good high temperature stability and oxidation resistance.
Incoloy 800H is a nickel-iron-chromium alloy, which is an improved version of 800 alloy and has a series of excellent physical and chemical properties. The following is a detailed description of Incoloy 800H material:
The main chemical components of Incoloy 800H include nickel (Ni), iron (Fe), chromium (Cr), aluminum (Al) and titanium (Ti), among which:
The nickel (Ni) content is between 30.0% and 35.0%.
The iron (Fe) content is at least 39.5%.
The chromium (Cr) content is between 19.0% and 23.0%.
The aluminum (Al) content is between 0.15% and 0.60%.
The carbon (C) content is between 0.15% and 0.60%.
Ni | Fe | Cr | Al | C |
30.0%- 35.0%. | ≥39.5% | 19.0%- 23.0%. | 0.15% -0.60%. | 0.15% - 0.60%. |
In addition, the alloy also contains a small amount of manganese (Mn), sulfur (S) and phosphorus (P), among which the maximum manganese (Mn) content is 1.50%, and the sulfur (S) and phosphorus (P) contents do not exceed 0.015%. The reasonable combination of these elements gives Incoloy 800H alloy excellent oxidation resistance and corrosion resistance.
Physical properties
Density: 7.94 g/cm³.
Melting point: approximately between 1350-1400°C.
Elastic modulus: 205 GPa.
Tensile strength (room temperature, tensile strength): ≥ 450 MPa.
Yield strength (room temperature): ≥ 170 MPa.
Elongation (room temperature, fracture): ≥ 30%.
Performance characteristics
Anti-oxidation and corrosion resistance: In a high-temperature oxidizing environment, a dense oxide film can be formed on the surface of Incoloy 800H, which effectively resists oxidation and corrosion. It also has excellent corrosion resistance to nitric acid, organic acids, etc., but has limited corrosion resistance in sulfuric acid and hydrochloric acid.
High-temperature strength and corrosion resistance: Incoloy 800H can maintain good mechanical properties and corrosion resistance at high temperatures, and is suitable for long-term use in high-temperature oxidizing environments.
High-temperature creep resistance: The alloy has excellent high-temperature creep resistance and can maintain stable shape and size at high temperatures.
Processing and welding performance: Incoloy 800H has good processing and welding performance, which can meet the requirements of various complex manufacturing processes. Conventional welding methods such as arc welding, TIG welding, MIG welding, etc. are applicable.
Application fields
Due to the excellent properties of Incoloy 800H alloy, it is widely used in the following fields:
Chemical industry: used to manufacture high-temperature equipment such as furnace tubes, furnaces, reactors, etc.
Energy industry: used to manufacture power plant boilers, heat exchangers and other equipment.
Oil processing: used to manufacture refinery equipment such as heating furnace tubes, regenerators, heat exchangers, etc.
Aerospace: In the aerospace field, Incoloy 800H is used to manufacture high-temperature components such as combustion chambers and turbine disks of turbine engines.
In summary, Incoloy 800H is a high-temperature alloy with excellent oxidation resistance, corrosion resistance and high-temperature strength, which plays an important role in many industrial fields.
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Other,Seller,Trading Company
Year Established:
2010
Total Annual:
1000000-1500000
Employee Number:
100~200
Ecer Certification:
Verified Supplier
Main Products stainless steel series 304, 304L, 321, 316L, 317L, 309s, 310s,904L,410, 420, 430, 441, 409, 436, 441, 439, 630,etc. Duplex stainless steel series 2205, 2507,etc. HastelloyC-276, B-2, C-2000,etc. Nickel-based alloy series Inconel625, 718, Incoloy825, 800H, Monel400,etc. Superalloy s... Main Products stainless steel series 304, 304L, 321, 316L, 317L, 309s, 310s,904L,410, 420, 430, 441, 409, 436, 441, 439, 630,etc. Duplex stainless steel series 2205, 2507,etc. HastelloyC-276, B-2, C-2000,etc. Nickel-based alloy series Inconel625, 718, Incoloy825, 800H, Monel400,etc. Superalloy s...
Get in touch with us
Leave a Message, we will call you back quickly!