| Density | ~8.9g/cm³ (0.321 lb/in³) |
| Melting Point | ~1350-1450°C (2460-2640°F) |
| Tensile Strength | ~900 MPa (130 ksi) |
| Yield Strength | ~750 MPa (109 ksi) |
| Elongation | ~15% |
| Thermal Conductivity | ~14 W/m·K (10 BTU·in/hr·ft²·°F) |
| Modulus of Elasticity | ~210 GPa (30 x 10³ ksi) |
| Corrosion Resistance | Good resistance to oxidation and corrosion at high temperatures |
| Applications | Aerospace components, gas turbines, high-temperature industrial parts |
| Brand Name | Zhonggong Special Metallurgy |
| Model Number | GH39 Alloy |
| Place of Origin | China |
| Certification | ISO Certificate |
View Detail Information
Explore similar products
Nickel Alloy INCONEL600 Steel Plate N06600 Thin Plate Corrosion Resistant T3
High Strength INCONEL718 Alloy Steel Strip GH4169 Nickel Based Round Steel Rod
GH5188 Alloy Nickel Based Superalloy High Strength Oxidation Resistance
Gh3039 Corrosion Resistant Nickel Based Superalloy 8.23 g/cm3 high performance
Product Specification
| Payment Terms | Payment Terms: Mainly T/T.. L/C, D/A, D/P, | Supply Ability | 5000 tons per month |
| Delivery Time | 5-8 working days, depending on the parameters required for negotiation | Packaging Details | Standard export packaging, or packaging as required |
| Density | ~8.9g/cm³ (0.321 lb/in³) | Melting Point | ~1350-1450°C (2460-2640°F) |
| Tensile Strength | ~900 MPa (130 ksi) | Yield Strength | ~750 MPa (109 ksi) |
| Elongation | ~15% | Thermal Conductivity | ~14 W/m·K (10 BTU·in/hr·ft²·°F) |
| Modulus of Elasticity | ~210 GPa (30 x 10³ ksi) | Corrosion Resistance | Good resistance to oxidation and corrosion at high temperatures |
| Applications | Aerospace components, gas turbines, high-temperature industrial parts | Brand Name | Zhonggong Special Metallurgy |
| Model Number | GH39 Alloy | Place of Origin | China |
| Certification | ISO Certificate | ||
| High Light | GH39 Nickel Based Superalloy ,Anti Oxidation Nickel Based Superalloy | ||
GH39 Alloy is a high-performance nickel-based superalloy engineered for exceptional strength and oxidation resistance at elevated temperatures. It is specifically designed to perform reliably in extreme environments, making it ideal for aerospace and industrial applications where high thermal and mechanical stress is common.
Key Properties and Features:
High-Temperature Strength: GH39 Alloy maintains excellent mechanical properties at elevated temperatures, with high tensile strength (~900 MPa or 130 ksi) and yield strength (~750 MPa or 109 ksi). It is capable of withstanding temperatures up to approximately 1350-1450°C (2460-2640°F) without significant loss of strength.
Oxidation and Corrosion Resistance: The alloy exhibits superior resistance to oxidation and high-temperature corrosion, ensuring long-term durability and performance in harsh environments. This property is crucial for applications in gas turbines, jet engines, and other high-temperature processes.
Mechanical Properties: GH39 provides good elongation (~15%), which enhances its ability to handle mechanical stresses and strains without failure, contributing to structural integrity in demanding applications.
Thermal Conductivity: With a thermal conductivity of approximately 14 W/m·K (10 BTU·in/hr·ft²·°F), GH39 effectively manages heat, helping to maintain thermal stability and reduce overheating in high-performance systems.
Applications: Commonly used in aerospace components, high-temperature gas turbines, and other industrial applications requiring high strength, oxidation resistance, and thermal stability. GH39’s robust performance in extreme conditions ensures it is a reliable choice for advanced engineering tasks.
GH39 Alloy's combination of high strength, excellent oxidation resistance, and thermal stability makes it a preferred material for critical applications where reliability and durability are paramount.
Here’s a composition table for GH39 Alloy:
| Element | Composition Range (%) |
|---|---|
| Nickel (Ni) | 60.0 - 65.0 |
| Chromium (Cr) | 15.0 - 20.0 |
| Cobalt (Co) | 5.0 - 10.0 |
| Molybdenum (Mo) | 3.0 - 5.0 |
| Iron (Fe) | ≤ 6.0 |
| Titanium (Ti) | 1.0 - 2.0 |
| Aluminum (Al) | 1.0 - 2.0 |
| Carbon (C) | ≤ 0.10 |
| Manganese (Mn) | ≤ 0.5 |
| Silicon (Si) | ≤ 0.5 |
| Sulfur (S) | ≤ 0.01 |
These values are general guidelines. For precise specifications or detailed applications, consult specific standards or suppliers.
![]()
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Other,Seller,Trading Company
Year Established:
2010
Total Annual:
1000000-1500000
Employee Number:
100~200
Ecer Certification:
Verified Supplier
Main Products stainless steel series 304, 304L, 321, 316L, 317L, 309s, 310s,904L,410, 420, 430, 441, 409, 436, 441, 439, 630,etc. Duplex stainless steel series 2205, 2507,etc. HastelloyC-276, B-2, C-2000,etc. Nickel-based alloy series Inconel625, 718, Incoloy825, 800H, Monel400,etc. Superalloy s... Main Products stainless steel series 304, 304L, 321, 316L, 317L, 309s, 310s,904L,410, 420, 430, 441, 409, 436, 441, 439, 630,etc. Duplex stainless steel series 2205, 2507,etc. HastelloyC-276, B-2, C-2000,etc. Nickel-based alloy series Inconel625, 718, Incoloy825, 800H, Monel400,etc. Superalloy s...
Get in touch with us
Leave a Message, we will call you back quickly!